Stainless Steel Alloy 403 is a straight chromium stainless steel that demonstrates reasonable corrosion resistance, high mechanical characteristics, and offers heat resistance and a scaling temperature of about 1300°F. 304 is corrosion and heat resistant martensitic stainless steel that offers a wide range of mechanical properties obtainable by appropriate heat treating. Easily hardened by oil, fan or air cooling and can be tempered at temperatures at 1350°F (732°C) to improve fracture toughness.
Stainless Steel product forms offered at all Titanium Industries’ locations:
Stainless Steel Alloy 403 Applications:
- Compressor blades
- Turbine parts
DISCLAIMER: Alloy data sheets are for reference only, not for design purposes.
Chemical Composition | |||||||||
---|---|---|---|---|---|---|---|---|---|
Cr 11.5 – 13.0% | Ni 0.60% Min | C 0.15% Max | Si 0.50% Max | Mn 1.0% Max | |||||
P 0.04% Max | S 0.03% Max | Fe Balance |
PHYSICAL PROPERTIES | ||||||
---|---|---|---|---|---|---|
Density | Electrical conductivity (% IACS) | Thermal conductivity (BTU/lbm -°F) | Specific heat capacity (BTU/lbm -°F) | Thermal expansion (min/in)-°F | Melting Point (°F) | |
0.276 | – | 9.3 | 14.4 | 6.6 | – |
Mechanical Properties | |||||||||
---|---|---|---|---|---|---|---|---|---|
Property | Minimum | Maximum | |||||||
Yield Strength Range (Rp0.2 Offset) (ksi) | – | 45 | |||||||
Tensile Strength Range (Rm) (ksi) | – | 70.3 | |||||||
Elongation (AL=5 x Ø) | – | 25.0% | |||||||
Brinell Hardness (H) | – | 139 | |||||||
Modulus of Elasticity (ksi) (E): 30458 | |||||||||
Machineability General Index: – |